Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60112 |
RedEye On Demand ABS for Rapid Prototyping ABS or Acrylonitrile butadiene styrene is a true industrial thermoplastic that is impact-resistant and structurally strong. ABS parts are built with a layered manufacturing process utilizing Fused D.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | |
LG Chemical HI100K ABS, High Impact Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60243 |
Solvay TECHNYL® A 238 Black 21 N PA66, Conditioned Description: Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 238 offers excellent .. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60243 |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, DRY Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Dielectric Strength | 32.0 kV/mm @Thickness 1.00 mm |
813 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Unitika A125 PA66, Dry Information provided by Unitika Ltd. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60250 |
Polyram PlusTek PA801 Nylon 6.6 Copolymer for Injection Molding, Impact Modified Impact modified Nylon 6.6 copolymer for injection molding application.Information provided by Polyram. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® 2D 20 nat PA612 Product Description: Grilamid 2D 20 natural is an unmodified unreinforced, medium viscosity polyamide 612 (PA612), designed for injection molding as well as extrusion. It is characterized by the fol.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® B 70 GFE 15 H PA6-GF15 Product description: Grilon B 70 GFE 15 H is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon B 70 GFE 15 H has the following important prop.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 16 GM nat PA12 Grilamd L16 GM is a low-viscosity, non-reinforced PA 12 grade, UV- and heat-stabilized. The modification with a crystallization regulator causes a quick freeze and a fine, crystalline structure. Due.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 16 LM PA12 Product Description: Grilamid L 16 LM is a , low viscosity extrusion type, based on Polyamide 12 (PA12). Grilamid L 16 LM is UV- and heat stabilized. The modification with a nucleation agent results.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 20 HL black 9563 PA12 Product Description: Grilamid L 20 HL black 9563 is a, medium viscosity extrusion grade, based on Polyamide 12 (PA12). Grilamid L20 HL black 9563 has been especially developed for external cable she.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 25H FWA nat PA12 Product Description: Grilamid L 25 H FWA natural is a highviscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 25 H FWA natural is designed for technical injection moulded com.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | AC Rapid Rise; ASTM D149 |
DuPont™ Nomex® 410 Paper, 10 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | AC Rapid Rise; ASTM D149 |
DuPont™ Nomex® 410 Paper, 12 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4095 black 9225 PA*-GF50 Product description: Grivory XE 4095 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60243-1 |
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)
(Unverified Data**) 45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60243-1 |
DuPont Performance Polymers Rynite® 530 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength stiffness and toughness excellent .. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60243-1 |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT) Unreinforced Renewably Sourced Polytrimethylene Terephthalate with Excellent Impact Resistance Sorona MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 20H FWA nat PA12 Product Description: Grilamid L 20 H FWA natural is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA natural is used for technical injection molded parts.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 22A W 40 X PA12-I Product Description: Grilamid L 22A W 40 X is a flexible plasticized and impact modified heat and light stabilized Polyamide 12 (PA12). The main features of Grilamid L 22A W 40 X are: Good impact st.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 25 W 40 NZ PA12-I Product Description: Grilamid L 25 W 40 NZ is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 NZ is impact modified and heat and UV stabilized. The.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 243-1 |
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced 50% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | in transformer oil; IEC 60243-1 |
CENTROPLAST CENTROMID 12 Polyamide 12 This extruded material has good impact resistance, low moisture absorption and good chemical resistance. It is used in precision elements, drive parts, cases and housingsInformation provided by CEN.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60243 |
Teijin Panlite® LD-1000RM High Light Reflection Polycarbonate Resin Polycarbonate-resin-base good light-reflection grade. It exhibits high light-reflection (over 96 %) at whole visible light range and also light shut-out even at a thinner thickness portion.Applicati.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | CEI 60243-1 |
Addiplast Addinyl C2 ZV15 Nylon 66/6, 15% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TR 55 LZ PA12/MACMI Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LZ offers a variety of interesting properties such as: c.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TR 55 LY PA12/MACMI Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LY offers a variety of interesting properties such as: c.. |