Material Notes:
MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are platy, hydrophobic, non-abrasive and chemically inert. They provide an excellent balance of properties in a number of industrial applications in addition to paint & coating, such as adhesives & sealants, mastics, joint compounds and other construction product applications.Information provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Specific Gravity 2.78 g/cc
2.78 g/cc
Bulk Density 0.368 g/cc
0.0133 lb/in³
Loose
0.945 g/cc
0.0341 lb/in³
Tapped
Brightness 86 %
86 %
Hunter Rd, Dry
Oil Absorption 27 %
27 %
g oil/100 g filler; ASTM D281
Moisture Absorption at Equilibrium 0.50 %
0.50 %
Loss On Ignition 8.0 %
8.0 %
Particle Size 1.5 µm
1.5 µm
@ 10%
7.0 µm
7.0 µm
D50
15 µm
15 µm
@ 90%
Particle Mesh Size 325 Mesh
325 Mesh
0.1% retained
pH 8.7
8.7
Component Elements Properties Metric English Comments
Al2O3 <= 1.5 %
<= 1.5 %
CaO <= 1.5 %
<= 1.5 %
Fe2O3 <= 1.5 %
<= 1.5 %
MgO 30 %
30 %
SiO2 60 %
60 %
Users viewing this material also viewed the following: