Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.368 g/cc | 0.0133 lb/in³ | loose |
Nyco NYAD® G Special Wollastonite Wollastonite (calcium metasilicate, or CaSiO3) is a naturally occurring white, non-metallic mineral with an acicular or needle-shaped crystal structure. This distinctive property makes wollastonite .. |
|||
Bulk Density | 0.368 - 0.449 g/cc | 0.0133 - 0.0162 lb/in³ | Loose |
KaMin KaMin® 70C Kaolin Clay - Calcined High brightness, work-horse calcined kaolin clay, extremely low crystalline silica content.Industry: Paint & Coatings, Adhesives & SealantsUses: Architectural Coatings, Industrial Coatings, Flat/Mat.. |
|||
Bulk Density | 0.368 - 0.449 g/cc | 0.0133 - 0.0162 lb/in³ | Loose |
KaMin Polyfil® 70 Kaolin Clay - Calcined Calcined clays, such as Polyfil® 70, are brighter than most water-washed clays, offering excellent processing and limited reinforcement. They impart outstanding wet/dry electrical properties due .. |
|||
Bulk Density | 0.368 - 0.449 g/cc | 0.0133 - 0.0162 lb/in³ | Loose |
KaMin Polyfil® 80 Kaolin Clay - Calcined Higher brightness, medium particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber GoodsInformation provided by KaMin LLC. |
|||
Bulk Density | 0.368 g/cc | 0.0133 lb/in³ | Loose |
CIMBAR CIMTUFF® 9107 Talc CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® .. |
|||
Bulk Density | 0.368 g/cc | 0.0133 lb/in³ | Loose |
CIMBAR Gel Talc for Polyester Filler Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyes.. |
|||
Bulk Density | 0.368 g/cc | 0.0133 lb/in³ | Loose |
CIMBAR MV 607 Talc MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla.. |
|||
Bulk Density | 0.368 g/cc | 0.0133 lb/in³ | Loose |
CIMBAR RP 9305 Talc RP 9300 Series talcs are produced from high purity ores, which provide an excellent balance of color and mechanical properties, for primary use in commodity polypropylene and polyester compounds. R.. |