Material Notes:
Seaboard DS is a high density polyethylene (HDPE) foam core product with a specially formulated skin to add stiffness and Dimensional Stability. This new product from Compression Polymers combines light weight, economy, and superior strength in a foam core product. Seaboard DS is ideal for applications where additional stiffness and strength are required such as, engine covers, seat backs and bottoms, instrument panels, tackle storage etc.FEATURES AND BENEFITS Strength- Seaboard DS is stronger than standard foam core materials. Stiffness- Seaboard DS is stiffer to provide additional support for seat and engine cover applications. UV Stability- Seaboard DS is UV stabilized to withstand the elements. Dimensionally Stable- Seaboard DS has a unique skin that provides lower shrink rates and repeatable dimensions.Information provided by Compression Polymers Corp - Vycom
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 25 hour
25 hour
F50; ASTM D1693
>= 500 hour
>= 500 hour
F50; ASTM D2561
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
ASTM D2240
Flexural Strength 49.6 MPa
7200 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.9 °C
183 °F
ASTM D648
Vicat Softening Point 130 °C
266 °F
ASTM D1525
Brittleness Temperature -76.1 °C
-105 °F
ASTM D746