Carmel Olefins CAPILENE® SR 50 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CAPILENE® SR 50 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CAPILENE® SR 50 is a medium melt flow rate impact copolymer for injection molding applications. This grade offers good balance of stiffness, impact strength and processability.Applications: Typical applications of CAPILENE® SR 50 are packaging, household articles and automotive parts.Information provided by Carmel Olefins.
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
50 mm/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
50 mm/min; ASTM D638
Flexural Modulus 1.15 GPa
167 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm

@Temperature -20.0 °C
0.937 ft-lb/in

@Temperature -4.00 °F
ASTM D256
0.950 J/cm

@Temperature 23.0 °C
1.78 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648
Vicat Softening Point 150 °C

@Load 1.02 kg
302 °F

@Load 2.25 lb
ASTM D1525