Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.15 GPa | 167 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PC 69 T 10 003/1M Polypropylene reinforced with mineral filler Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PQ 82 N 003/1M Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | Tangent; 1.3 mm/min; ASTM D790 |
Mytex Polymers AN16L-53 Polypropylene, Compounded Description: Compounded polypropylene produced for automotive exterior applications using Mytex® Technology.Key Applications: Body side moldingInformation provided by Mytex Polymers |
|||
Flexural Modulus | >= 1.15 GPa | >= 167 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 6751E (516H5) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | >= 1.15 GPa | >= 167 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 6752G (526H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | >= 1.15 GPa | >= 167 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 8348S (EPH31RA) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | >= 1.15 GPa | >= 167 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 8300G (EPYS30RE) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | >= 1.15 GPa | >= 167 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 8340S (EPYH31U) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GM 8260 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
MRC Polymers MAXTEL™ 600T18-UV TPO, 18% Talc Filled, UV Stabilized • For automotive exterior applications• Excellent process ability and dimensional stabilityInformation provided by MRC Polymers Inc. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
Iran Petrochemical (PCC) EP-T 30 R Polypropylene The grade is a medium flow heterophasic the copolymer mainly designed for injection molding application.Application: containers, buckets, pails, crates and also used for automotive parts.Informatio.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY 63000CTC PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® HD 5211 EA HDPE Injection Molding Applications:Paint pailsBottle capsHouse waresToysInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | 2mm/min; ISO 178 |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
Unipetrol PP MONSTEN® MA 611 Polypropylene Impact Copolymer Made for injection molding applications. Antistatic stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 527-2 |
Total PPC 11712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 11712 is a nucleated controlled-rheology heterophasic copolymer. PPC 11712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 527-2 |
Total PPC 3660 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 3660 is an heterophasic copolymer. PPC 3660 is characterized by a low fluidity hence good melt strength to provide east of processing and good manufactured article propert.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ASTM D 790 |
Total PPC 4624WZ Polypropylene, Impact Copolymer ATOFINA 4624WZ polypropylene is a nucleated impact copolymer, combining good fluidity and mechanical properties. 4624WZ is characterized by significantly improved resistance, while maintaining exce.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
Total PPR 10222 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 10222 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
Total PPR 10232 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 10232 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
Total PPR 12232 Random Copolymer Polypropylene Total Petrochemicals PPR 12232 is a high melt flow index, high transparency random copolymer. Its has an excellent food compatibility due to its low odor, making it especially suitable for the produ.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | At 2 mm/min; ISO 178 |
Borealis Daplen™ EE015U TPO Compound Daplen EE015U is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE015U is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
Total PPC 3650 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 3650 is a heterophasic copolymer with a Melt Flow index of 2 g/10 min.Polypropylene PPC 3650 provides an excellent balance between toughness and flow, being particularly suitable i.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ASTM D790 |
Equate EMDA-8920 HDPE Injection Molding Resin EMDA-8920 is a high density copolymer polyethylene resin designed for injection molding applications which require excellent toughness and gloss.Applications: EMDA-8920 is a high density copolymer p.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | SAE J949 |
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness) AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ASTM D790 |
Carmel Olefins CAPILENE® SE 50 E Polypropylene Impact Copolymer Description: CAPILENE® SE 50 E is a low melt flow rate impact copolymer intended for sheet extrusion. It exhibits excellent impact strength even at low temperatures, combined with good processabi.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO Data |
BASF Ultramid® 1003-2 NF2002 PA66 (Conditioned) Ultramid 1003-2 NF2002 is a general purpose, heat stabilized nylon 6/6. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXFLEX® 925 TPO
(discontinued **) Description: DEXFLEX® 925 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and e.. |