Material Notes:
SL 200 ST is a silicon nitride ceramic especially suitable for components exposed to mechanical stress and engine-specific applications even at elevated temperatures. It is recognized for its high strength and crack resistance, as well as its resistance to sudden changes in temperature. In contrast to the other silicon nitride materials, this is a gas-pressure sintered Si3N4 and hence possesses much better mechanical properties such as greater flexural strength, fracture toughness, and a higher Weibull modulus.
Physical Properties Metric English Comments
Density 3.21 g/cc
0.116 lb/in³
DIN EN 623-2 / ASTM-C373 / ASTM-C20
Water Absorption 0.00 %
0.00 %
DIN EN 623-2 / ASTM-C373
Permeability 0.00
0.00
Gas
Weibull Modulus 15
15
DINV ENV 843-5
Mechanical Properties Metric English Comments
Vickers Microhardness 1500
1500
HV 0.5; DINV ENV 843-4
Tensile Strength at Break 750 MPa
109000 psi
ACMA Test #4 / DIN EN 843-1
Tensile Modulus 305 GPa
44200 ksi
Young's; DINV ENV 843-2 / ASTM-F417
Flexural Strength 900 MPa
131000 psi
DIN EN 843-1
Compressive Strength 3000 MPa
435000 psi
ASTM C-773-88 / DIN 51067T1
Poissons Ratio 0.26
0.26
DINV ENV 843-2
Fracture Toughness 7.00 MPa-m½
6.37 ksi-in½
DIN 51109
Shear Modulus 121 GPa
17500 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 3.20 µm/m-°C

@Temperature 20.0 - 200 °C
1.78 µin/in-°F

@Temperature 68.0 - 392 °F
DIN EN 821-1
4.30 µm/m-°C

@Temperature 20.0 - 1000 °C
2.39 µin/in-°F

@Temperature 68.0 - 1830 °F
DIN EN 821-1
Specific Heat Capacity 0.700 J/g-°C

@Temperature 100 - 200 °C
0.167 BTU/lb-°F

@Temperature 212 - 392 °F
DINV ENV 821-3
Thermal Conductivity 21.0 W/m-K

@Temperature 20.0 - 100 °C
146 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
DIN EN 821-2 / ASTM-C408
Maximum Service Temperature, Air 1300 °C
2370 °F
Maximum Service Temperature, Inert 1600 °C
2910 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM-D257
Dielectric Constant 8.0

@Frequency 1.00e+6 Hz
8.0

@Frequency 1.00e+6 Hz
IEC 672-1 / ASTM-C150
Dielectric Loss Index 0.00010

@Frequency 1.00e+9 Hz
0.00010

@Frequency 1.00e+9 Hz
IEC 672-1 / ASTM-D149,150