Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
GrafTech eGRAF® SPREADERSHIELD™ SS1500 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
GrafTech eGRAF® SPREADERSHIELD™ SS300 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
GrafTech eGRAF® SPREADERSHIELD™ SS400 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
GrafTech eGRAF® SPREADERSHIELD™ SS500 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
GrafTech eGRAF® SPREADERSHIELD™ SS600 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Specific Heat Capacity 0.700 J/g-°C

@Temperature 0.000 - 50.0 °C
0.167 BTU/lb-°F

@Temperature 32.0 - 122 °F
Momentive Performance Materials Type 219 Fused Quartz Tubing
Known as "Ozone-Free" or "Germicidal" quartz tubing. Transmits UV-A and UV-B while blocking the deep, high energy wavelengths that cause ozone generation and pose the greatest exposure risks. Tran..
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
Skamol Group ISOPERLOR 550P Perlite Insulating Brick & Block
ISOPERLOR perlite insulating bricks & blocks have the following characteristics: Max. service temperature 900°C (1652°F)Back-up insulation onlyExcellent insulating propertiesVery lightweight a..
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
Skamol Group Moler HIPOROS Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Specific Heat Capacity 0.700 J/g-°C

@Temperature 100 - 200 °C
0.167 BTU/lb-°F

@Temperature 212 - 392 °F
DINV ENV 821-3
CeramTec 701 Cordierite
Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c..
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
DINV ENV 821-3
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2
DC 25 is a ZTA Alumina Zirconia Platelet Composite used in dental applications.
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
DINV ENV 821-3
CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3
SL 200 BG is a silicon nitride ceramic used to make welding rollers, pins, and components, gas nozzles, and forming tools. Silicon nitrides are ideal for components working under mechanical loads an..
Specific Heat Capacity 0.700 J/g-°C

@Temperature 100 - 200 °C
0.167 BTU/lb-°F

@Temperature 212 - 392 °F
DINV ENV 821-3
CeramTec SL 200 ST Silicon Nitride, Si3N4-Y2O3
SL 200 ST is a silicon nitride ceramic especially suitable for components exposed to mechanical stress and engine-specific applications even at elevated temperatures. It is recognized for its high s..
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
DINV ENV 821-3
CeramTec SL 303 Silicon Nitride, SiAION+SiC
SL 303 is a silicon nitride ceramic. Silicon nitrides are ideal for components working under mechanical loads and engine parts, even and especially at elevated temperatures. Their property profile i..
Specific Heat Capacity 0.700 J/g-°C

@Temperature 100 - 200 °C
0.167 BTU/lb-°F

@Temperature 212 - 392 °F
DINV ENV 821-3
CeramTec 192/193 Titania
192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra..
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
ASTM E1269
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2)
Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
silicone property; ASTM E 1461-1
Arlon Thermabond® 99000W008 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
silicone property; ASTM E 1461-1
Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
E 1461-01
Arlon Thermabond® R36300W008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Low Outgassing, Thermally Conductive, Electrically Insulating, Thermabond® Bonds without primerRecommended Primers: Dow Corning S2260Design/Construction: Liner: FEP Product: Uncured S..
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
E 1461-01
Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical val..
Specific Heat Capacity 0.700 J/g-°C

@Temperature 100 - 200 °C
0.167 BTU/lb-°F

@Temperature 212 - 392 °F
DINV ENV 821-3
CeramTec 447 Cordierite, 2MgO•Al2O3•5SiO2
Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c..
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
CeramTec 547 Cordierite (2MgO-2Al2O3-5SiO2)
Te value is 670°C. Hasselman Thermal Shock value is 800 K.Data provided by CeramTec North America.
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
CeramTec 965 Toughened Alumina (Al2O3-ZrO2)
Hasselman Thermal Shock value is 270 K.Data provided by CeramTec North America.