Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.20 g/cc | 0.116 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 113 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
NanoScale NanoActive® Magnesium Oxide NanoActive MgO is produced using proprietary processes to obtain high specific surface area, small crystallite size material possessing high chemical reactivity, particularly at elevated temperature.. |
|||
Density | >= 3.20 g/cc | >= 0.116 lb/in³ | |
MarkeTech AN 90 Aluminum Nitride Ceramic Substrate, 98% Purity Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in.. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 Â.. |
|||
Density | 3.20 - 3.65 g/cc | 0.116 - 0.132 lb/in³ | |
MarkeTech MC-LD and MC-MD Ultra High Temperature Machinable Ceramics For very high temperatures or where thermal conductivity or thermal shock is important, these machinable alkaline/alkaline earth zirconium phosphate ceramics (NaZr2P3O12 or BaZr4P6O24) are recommend.. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
MMCC Al/Al2O3 Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
Mo-Sci Corporation GAI-40-N Green A Intruder Filter Glass Applications: Lead-free NVIS Intruder Green A filter glass for Nichia White LED sources.Information provided by Mo-Sci Corporation. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
Mo-Sci Corporation WB-40-N White B Filter Glass Applications: Lead-free NVIS White class B filter glass for white LED sources.Information provided by Mo-Sci Corporation. |
|||
Density | 3.22 g/cc | 0.116 lb/in³ | |
Schott GG385 Long Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630.. |
|||
Density | 3.22 g/cc | 0.116 lb/in³ | |
Schott WG320 Long Pass Filter Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66.. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
Schott N-BASF64 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
Schott N-KZFS11 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.22 g/cc | 0.116 lb/in³ | |
Schott N-SF11 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Compression Moldings Glass-mica compound that occupies a place between plastics and ceramics in terms of usage temperature. It can be molded and machined like plastics and has the mechanical properties (strength, hardn.. |
|||
Density | 3.21 g/cc | 0.116 lb/in³ | DIN EN 623-2 |
CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3 SL 200 BG is a silicon nitride ceramic used to make welding rollers, pins, and components, gas nozzles, and forming tools. Silicon nitrides are ideal for components working under mechanical loads an.. |
|||
Density | 3.21 g/cc | 0.116 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec SL 200 ST Silicon Nitride, Si3N4-Y2O3 SL 200 ST is a silicon nitride ceramic especially suitable for components exposed to mechanical stress and engine-specific applications even at elevated temperatures. It is recognized for its high s.. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
Trelleborg Emerson & Cuming Eccobond® 64C Two-Component Nickel Filled Electrically Conductive Epoxy Adhesive Emerson & Cuming 64C Eccobond® Two-Component Nickel Filled Electrically Conductive Epoxy AdhesiveTwo component, nickel filled, electrically conductive epoxy adhesive. Room temperature cure. Good ba.. |
|||
Density | 3.21 g/cc | 0.116 lb/in³ | ASTM C20 |
CoorsTek Pure SiC™ HR CVD Silicon Carbide, > 99.9995% Data Provided by the manufacturer, CoorsTek, Inc. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | Apparent density (SiC outer layer) |
Destech Silicon Carbide, Solid or Foamed Destech silicon carbide foam is produced by chemical vapor reaction (CVR), in which high temperature silicon bearing gases convert glassy, or vitreous, carbon foam to SiC. Destech SiC foam has no c.. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN SM-B40 PTFE Reinforced with 40% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
Arlon TC600 Glass, PTFE and Micro-Dispersed Ceramic High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED). |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
Ceradyne CeraTrex™ SC-P2 Silicon Carbide Features:purity>99.9995%corrosion resistancewear resistancenear net shape fabrication to 400 mm OD Applications:semiconductor componentswear componentsInformation provided by Ceradyne Company |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | A Component; ASTM D1475 |
Aptek 2210A/B Electrically conductive urethane adhesive Electrically conductive urethane adhesive, silver-filled, flexible low modulus, low outgassingAPTEK 2210-A/B is a two component, silver-filled, urethane adhesive designed for application where flexi.. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | ASTM D792 Method A |
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist.. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
Parker Chomerics CHO-BOND 1024 Conductive Silicone Splicing Compound Conductive splicing compounds are intended for making "custom" EMI/RFI gaskets from standard CHO-SEAL® and CHO-SIL® strips. Compounds consist of Chomerics silver-bearing powders dispersed in silic.. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
Ceradyne Ceralloy® 147-31N Sintered Reaction Bonded Silicon Nitride (Si3N4) Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met.. |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
Ceradyne CeraTrex™ 146-S5 Silicon Carbide Features:corrosion resistancewear resistancehardnessnet shape fabricationApplications:wear componentsInformation provided by Ceradyne Company |
|||
Density | 3.20 g/cc | 0.116 lb/in³ | |
Mo-Sci Corporation YB-40-I Yellow B Filter Glass Applications: Lead-free NVIS Yellow class B filter glass for incandescent light sources.Information provided by Mo-Sci Corporation. |