Material Notes:
Navy IV typeModified barium titanates are widely used in transducers requiring moderate power level and receiving sensitivity. Special characteristics have made barium titanate a proven material for use in devices such as depth sounders and expendable hydrophones.Uses of this grade include: Low Power Sonar; High Power Sonar; Depth SoundersData provided by Channel Industries, Inc.
Physical Properties Metric English Comments
Density >= 5.55 g/cc
>= 0.201 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 21.0 MPa
3050 psi
Dynamic tensile strength
52.0 MPa
7540 psi
Static
Electrical Properties Metric English Comments
Curie Temperature >= 115 °C
>= 239 °F
Dielectric Constant 1350
1350
Free dielectric constant K<sup>T</sup><sub>3</sub>
1450
1450
K<sup>T</sup><sub>1</sub>
Dissipation Factor 0.0080
0.0080
Low Field
Piezoelectric Longitudinal Coupling Factor, k33 0.45
0.45
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -56.0
-56.0
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 245
245
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 12.2
12.2
Piezoelectric Planar Coupling Factor, kp -0.300
-0.300
Piezoelectric Mechanical Q 600
600
Piezoelectric Shear Coupling Factor, k15 0.45
0.45
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 145
145
Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N -4.70
-4.70
Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N 19.1
19.1
Piezoelectric Transverse Coupling Factor, k31 -0.180
-0.180