Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Chemlon 100 Nylon 66, Lubricated GP

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Chem Polymer
Trade Name Chemlon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 100 Nylon 66, Lubricated GP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A medium viscosity, general purpose injection molding grade nylon 66. Internally lubricated for excellent feed and mold release properties.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 83.0 MPa
12000 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Yield Strength 114 MPa
16500 psi
ASTM D790
Flexural Modulus 2.90 GPa
421 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ASTM D648
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Melt Temperature 271 °C
520 °F
Users viewing this material also viewed the following: