Chevron Phillips 1025 Extrusion Coating Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips 1025 Extrusion Coating Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Speed Resin, Base Resin Type - Chevron PE1017Characteristics: Excellent Processability at 570-620°F (300-325°C) Melt, Good Adhesion at Low Coating Weights and High Speed Lines, Low COF uses, FDA Approved for Food ContactApplications:Can be used in the outer coextrusion layer or monolayer coating for high slip applicationsData provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D1505-60T
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238-57T
Processing Properties Metric English Comments
Melt Temperature 299 - 327 °C
570 - 621 °F
Excellent Processability