Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips 5622 LDPE Shrink and Heavy Duty Packaging Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips 5622 LDPE Shrink and Heavy Duty Packaging Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: HomopolymerCharacteristics: Excellent Tensile and Impact Strength, Very Good Abrasion and Tear Resistance, Excellent Retention of Properties after Aging, Wide Range of Shrinkage Characteristics, No Slip and Low AntiblockApplications:Pallet Shrink, Heavy Duty PackagingProcessing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 2:1.Film properties below based on film thickness of 31.8 µm.Data provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM D1505
Melt Flow 0.50 g/10 min
0.50 g/10 min
Condition E; ASTM D 1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.170 GPa
24.7 ksi
ASTM D882
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Coefficient of Friction 0.50
0.50
ASTM D1894
Dart Drop 2.80 g/micron
71.1 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
ASTM D2457
Gloss 57 %
57 %
at 45°. ASTM D 2457
90 %
90 %
at 60°. ASTM D 2457
Processing Properties Metric English Comments
Melt Temperature 204 °C
399 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved