Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips HiD® 9035 HDPE Injection Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips HiD® 9035 HDPE Injection Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceApplications:Thin Wall Food Containers, ToysData provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D1505
Apparent Bulk Density 0.590 g/cc
0.0213 lb/in³
ASTM D1895
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
High Load Melt Index 1040 g/10 min

@Load 21.6 kg,
Temperature 190 °C
1040 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.4 MPa
3390 psi
ASTM D638
Elongation at Break <= 100 %
<= 100 %
ASTM D638
Flexural Modulus 0.970 GPa
141 ksi
3 pt. secant; ASTM D790
1.24 GPa
180 ksi
3 pt. Tangent; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 117 °C
243 °F
ASTM D1525