Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9035 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9055 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9062 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9402 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Homopolymer; Blow Molding, Sheeting and Profile ResinCharacteristics: High Melt Strength - Larger Parts, Wide Range of Processing Conditions, High Stiffness and Impact Resistance,.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9406 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good Parison Uniformity, Good Stress Crack ResistanceAppli.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9410 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good Parison Uniformity, Good TrimabilityApplications:Phar.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9412/HiD® 9413 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 99416 with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Homopolymer; Blow Molding, Sheeting & Profile Extrusion ResinCharacteristics: High Stiffness, Good Impact Resistance, Very Low Odor & Taste Transfer, Designated for Uniloy Blowmol.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9502/HiD® 9503 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Excellent ESCR, High Melt Strength, Good Impact Resistance.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9506 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good ESCR, High Melt Strength, Good Impact Resistance, Goo.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9075 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D3350 Classification 335540A; ASTM D4976 Classification: PE 235, A 54607Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, e.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9404 HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: medium molecular weight distributions, wide range of processing conditions, low parison sag, good stress crack resistance. Federal specification LP390C .. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9502H - 9503H High Performance Series HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: outstanding ESCR, excellent impact resistance, medium molecular weight distribution, wide range of processing conditions, high melt strength, good pariso.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips Marlex® 9506H High Performance Series HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: superior physical properties, medium molecular weight distribution, wide range of processing conditions, low parison sag, excellent stress crack resistan.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9706 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: moderate flow, good impact strength, excellent stiffness, good ESCR, moderate shrinkage resistanceApplications: crates and totes, structural foamInform.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9720 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: good flow, moderate impact strength, excellent stiffness, moderate ESCR, moderate shrinkage resistanceApplications: pails, structural foamInformation p.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips LX8119 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D4976 Classification: PE 233, A 56700Characteristics: warp resistant, excellent impact strength, excellent ESCR, moderate shrinkage resistanceApplications: seats, .. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | Average value: 0.590 g/cc Grade Count:14 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ISO 60 |
SolVin 250SB Polyvinyl Chloride General Purpose - Rigid Made by suspension polymerization.
APPLICATIONS
Injection : moldings with complex flow paths
Pressing : mixed with VC-VAc copolymers for gramophone records
Calendering : rigid films and sheets ; use.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips Marlex® 9006 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips Marlex® 9012 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 232, A 55600Characteristics: Good Flow, Good Impact Strength, Good Stiffness, Good ESCR, Good Shrinkage ResistanceApplications:Food Pails.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 232, A 53600Characteristics: Good Flow, Good Impact Strength, Good Stiffness, Good ESCR, Good Shrinkage ResistanceApplications:Housewares.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips Marlex® 9503HF High Performance Series HDPE Blow Molding Resin Resin Type: linear copolymerCharacteristics: outstanding ESCR, excellent impact resistance, medium molecular weight distribution, wide range of processing conditions, high melt strength, good pariso.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin Resin Type: linear copolymerCharacteristics: excellent physical properties, medium molecular weight distribution, wide range of processing conditions, good flow for injection blow molding applicatio.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips Marlex® 9708 HDPE Injection Molding Resin Resin Type: Linear Homopolymer; ASTM D 4976 Classification: PE 243, A 63700Characteristics: Moderate Flow, Good Impact Strength, Excellent Stiffness, Good ESCR, Moderate Shrinkage ResistanceApplicat.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 9512/HiD® 9513 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Apparent Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips LX8124 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D4976 Classification: PE 231, A 52600Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, excellent shrinkage resistanceApplic.. |
|||
Apparent Bulk Density | 0.590 - 0.610 g/cc | 0.0213 - 0.0220 lb/in³ | Average value: 0.595 g/cc Grade Count:17 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |