Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips MA5350 HIPS - High Impact Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips MA5350 HIPS - High Impact Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Rubber modified high impact polystyrene.Applications:Floppy diskettesDurable household applicationsThin to medium parts that require a combination of high gloss and good toughnessFeatures:Low coefficient of frictionVery high glossBalance of good impact and toughnessUL Classification 94HBInformation provided by Chevron PhillipsThe Chevron Phillips polystyrene product line was transferred to Americas Styrenics in 2008.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D-792
Bulk Density 0.609 - 0.673 g/cc
0.0220 - 0.0243 lb/in³
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
24 hours; ASTM D-955
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
2.0 in/min; 0.125" thickness; ASTM D-638
Elongation at Yield 48 %
48 %
2.0 in/min; 0.125" thickness; ASTM D-638
Tensile Modulus 2.27 GPa
329 ksi
2.0 in/min; 0.125" thickness; ASTM D-638
Flexural Strength 41.0 MPa
5950 psi
0.1 in/min; 0.250" thickness; ASTM D-790B
Flexural Modulus 2.24 GPa
325 ksi
0.1 in/min; 0.250" thickness; ASTM D-790B
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
2.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C

@Thickness 6.35 mm
183 °F

@Thickness 0.250 in
ASTM D-648
Vicat Softening Point 101 °C

@Thickness 6.35 mm
214 °F

@Thickness 0.250 in
Rate B; ASTM D-1525
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: