Chevron Phillips MarFlex® 1023 LDPE Extrusion Coating Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name MarFlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips MarFlex® 1023 LDPE Extrusion Coating Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Base, SpeedCharacteristics: Good adhesion at low coating weights and high line speedsLow COF usesFDA approved for food contactApplications: Can be used in the outer coextrusion layer or monolayer coating for high slip applicationsInformation provided by Chevron Phillips.
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D1505-60T
Melt Index of Compound 13 g/10 min
13 g/10 min
ASTM D1238-62T
Slip Level 1500 ppm
1500 ppm
Processing Properties Metric English Comments
Melt Temperature 299 - 327 °C
570 - 620 °F