Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips MarFlex® 9608XD HDPE Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name MarFlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips MarFlex® 9608XD HDPE Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This HDPE is tailored for applications that require:Very low gel levelsVery "clear" filmExcellent drawdownEnhanced stiffnessExcellent WVTR for a chill cast filmExcellent ProcessibilityTypical Cast Film Applications:CoextrusionsOverwrapFood packagingMoisture sensitive packagingProperty data based on 1.25 mil cast film.
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
ASTM D1505
Water Vapor Transmission 5.00 g/m²/day
0.322 g/100 in²/day
ASTM F1249
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 870 %
870 %
ASTM D882
Film Elongation at Break, TD 790 %
790 %
ASTM D882
Elmendorf Tear Strength, MD 1.38 g/micron
35.0 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 3.94 g/micron
100 g/mil
ASTM D1922
Dart Drop 1.38 g/micron
35.0 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 29.0 MPa
4210 psi
ASTM D882
Film Tensile Strength at Break, TD 23.0 MPa
3340 psi
ASTM D882
1% Secant Modulus, MD 758 MPa
110000 psi
ASTM D882
1% Secant Modulus, TD 841 MPa
122000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 11 %
11 %
ASTM D1003
Gloss 120 %
120 %
60°; ASTM D2457
Users viewing this material also viewed the following: