Material Notes:
Metallocene polyethylene antiblock masterbatch. This erucamide slip and antiblock concentrate with its mLLDPE carrier is tailored for use with mPACT™ resins in blown film applications that require: Reduced COFMinimal antiblock effect on opticsExcellent strengthApplications: Typical blown film applications include: Use with MarFlex™ D139 and MarFlex™ D143Recommended usage is 1 to 2%May also be used with conventional LLDPEInformation provided by Phillips
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
carrier resin value; ASTM D-1505
Melt Index of Compound 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
carrier resin value; ASTM D-1238
Antiblock Level 25 ppm
25 ppm
modified ASTM D-5630
Slip Level 50000 ppm
50000 ppm
modified ASTM; ASTM E-1252