Chevron Phillips Marlex® 9503H HDPE Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® 9503H HDPE Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Hexene CopolymerCharacteristics: Outstanding ESCRExcellent impact resistanceApplications: Detergent bottlesIndustrial containers/large partsHousehold and industrial chemical containersInformation provided by Chevron Phillips.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
Conditions A and B; ASTM D1693
Melt Index of Compound 0.31 g/10 min
0.31 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
2 in/min, Type IV bar; ASTM D638
Elongation at Break 500 %
500 %
2 in/min, Type IV bar; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
Tangent, 16:1 span:depth,0.5in/min; ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
Type A clamp, type 1 specimen; ASTM D746