Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® HHM 5502-01 Polyethylene, Sheet/Thermoforming Grade, HDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® HHM 5502-01 Polyethylene, Sheet/Thermoforming Grade, HDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Meets FDA Regulation 177.1520.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
Melt Flow 0.25 g/10 min
0.25 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Flexural Modulus 1.379 GPa
200.0 ksi
ASTM D790
Electrical Properties Metric English Comments
Dielectric Constant 2.33

@Frequency 100000 Hz
2.33

@Frequency 100000 Hz
ASTM D1531
Dielectric Strength 20.0 kV/mm

@Thickness 3.17 mm
508 kV/in

@Thickness 0.125 in
ASTM D149
Dissipation Factor >= 0.00010

@Frequency 100000 Hz
>= 0.00010

@Frequency 100000 Hz
ASTM D1531
Processing Properties Metric English Comments
Processing Temperature 149 - 177 °C
300 - 351 °F
Thermoforming surface
227 - 260 °C
441 - 500 °F
Extrusion
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved