ChevronTexaco Multifak® EP NLGI Grade 2

Category Fluid , Lubricant , Lithium Gellant
Manufacturer ChevronTexaco Corp
Trade Name Multifak® EP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Multifak® EP NLGI Grade 2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protection.Protection against shock loading, thus extending bearing life.Outstanding film strength.Good low temperature pumpability — Better handling in the container and grease dispensing equipment.Texaco Multifak EP greases are water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating greases.They are manufactured using highly refined, select high viscosity index base oils, and a lithium soap. They are brown in color and smooth and buttery in texture.Texaco Multifak EP greases are available in three grades:NLGI 0, 1 for better pumpability at low ambient temperatures.NLGI 2 for use in normal ambient temperatures.Texaco Multifak EP greases are formulated to:Protect bearings and other metal surfaces from corrosion when exposed to wet conditions.Resist water. These greases strongly resist being washed out of bearings.Retain their consistency under adverse service conditions.Provide outstanding film strength and adhesive properties. As a result, Texaco Multifak EP greases are particularly effective in providing low wear in shock load service.Operate effectively over a wide temperature range.Texaco Multifak EP greases are recommended for:General use in the lubrication of trucks, tractors, and passenger cars. This includes ball joints, universal joints, and all other chassis points, non-disc brake wheel bearings, water pumps, and fifth wheels.Boat trailer wheel bearings.Texaco Multifak EP 2 is approved for the NLGI Certification Mark LB.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication. Determined on mineral oil extracted by vacuum filtration.CPS Number: 220995; MSDS Number: 8644
Physical Properties Metric English Comments
Viscosity Measurement 90
90
Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 914 SUS
914 SUS
See Note 3.
Saybolt Viscosity at 210°F 82 SUS
82 SUS
See Note 3.
Kinematic Viscosity at 40°C (104°F) 173 cSt
173 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 15.6 cSt
15.6 cSt
See Note 3.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
Four Ball Wear 0.500 mm
0.0197 in
Scar Diameter
Penetration P(0), 1/10 mm 275
275
Unworked, 25°C (77°F)
Penetration P(60), 1/10 mm 280
280
Unknown Amount of Work, 25°C (77°F)
Timken Test 18100 g
40.0 lb
OK Load
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
See Note 2.
Minimum Service Temperature, Air -34.0 °C
-29.2 °F
See Note 1.
Pour Point -12.0 °C
10.4 °F
See Note 3.
Flash Point 198 °C
388 °F
See Note 3.
Dropping Point 188 °C
370 °F
Descriptive Properties Value Comments
Color Brown
Texture Buttery
Thickener, % 12
Lithium