China Tungsten STG70Cu-25 PM Structural Parts

Category Metal , Ferrous Metal
Manufacturer China Tungsten
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten STG70Cu-25 PM Structural Parts.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by China Tungsten
Physical Properties Metric English Comments
Density >= 6.20 g/cc
>= 0.224 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell <= 90
<= 90
Elongation at Break >= 0.50 %
>= 0.50 %
Component Elements Properties Metric English Comments
Carbon, C 0.50 - 0.80 %
0.50 - 0.80 %
Copper, Cu 2.0 - 4.0 %
2.0 - 4.0 %
Iron, Fe 93.7 - 96 %
93.7 - 96 %
Other 1.5 %
1.5 %
Descriptive Properties Value Comments
Impact Ductility (MPa), min 0.03