Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 - 0.017 cm/cm
0.012 - 0.017 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.3 MPa
10200 psi
ASTM D638
Elongation at Yield 25 %
25 %
ASTM D638
Flexural Yield Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Temperature 22.8 °C
0.900 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 224 °C
435 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
ASTM D648