Clariant Renol PA2SP0022 Nylon 6, Impact and Flow Modified, ESD Protection, Black

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol PA2SP0022 Nylon 6, Impact and Flow Modified, ESD Protection, Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Flexural Yield Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Temperature 22.8 °C
2.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+6 - 9.00e+9 ohm
1.00e+6 - 9.00e+9 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 243 - 279 °C
470 - 535 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm