Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Clariant Renol PPSSP0006 Polyphenylene Sulfide, Glass Fiber, PTFE Lubricated

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol PPSSP0006 Polyphenylene Sulfide, Glass Fiber, PTFE Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.62 g/cc
1.62 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 138 MPa
20000 psi
ASTM D638
Flexural Yield Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 9.65 GPa
1400 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Temperature 22.8 °C
1.10 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 299 - 321 °C
570 - 610 °F
Mold Temperature 51.7 - 79.4 °C
125 - 175 °F
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.000 - 0.345 MPa
0.000 - 50.0 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 50 rpm
20 - 50 rpm
Users viewing this material also viewed the following: