Clariant Renol PURSP0004 Thermoplastic Polyurethane, Ethylene Propylene Rubber Alloy

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol PURSP0004 Thermoplastic Polyurethane, Ethylene Propylene Rubber Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Processing Properties Metric English Comments
Melt Temperature 193 - 210 °C
380 - 410 °F
Mold Temperature 15.6 °C
60.0 °F
Dry Time 2 hour

@Temperature 65.6 °C
2 hour

@Temperature 150 °F
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 50 rpm
20 - 50 rpm