Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.40 MPa
348 psi
AVG Stress at Elongation M25; ASTM D412 Method A
Seals Eastern 7065 Neoprene / Chloroprene
General purpose neopreneInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 2.40 MPa

@Strain 100 %
348 psi

@Strain 100 %
ISO 527-1/-2
Covestro Desmopan® DP 9370A Polyurethane
Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission rateApplicationbreathable fi..
Tensile Strength, Yield 2.40 MPa

@Strain 100 %
348 psi

@Strain 100 %
ISO 527-1/-2
Covestro Desmopan® DP 9370AU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission r..
Tensile Strength, Yield 2.40 MPa

@Strain 100 %
348 psi

@Strain 100 %
Daikin DAI-EL G-752 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries.
Tensile Strength, Yield 2.40 MPa
348 psi
cured 72 hrs @ RT
ACC QM Skin 30 QSI Quantum Silicones 30 Durometer Condensation Cure moldmaking Material
QM Skin 30 is a two-component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and very low bleed in addition to good shelf-l..