Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.40 MPa | 348 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7065 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 2.40 MPa @Strain 100 % |
348 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 9370A Polyurethane Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission rateApplicationbreathable fi.. |
|||
Tensile Strength, Yield | 2.40 MPa @Strain 100 % |
348 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 9370AU Polyurethane Extrusion- and injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission r.. |
|||
Tensile Strength, Yield | 2.40 MPa @Strain 100 % |
348 psi @Strain 100 % |
|
Daikin DAI-EL G-752 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Tensile Strength, Yield | 2.40 MPa | 348 psi | cured 72 hrs @ RT |
ACC QM Skin 30 QSI Quantum Silicones 30 Durometer Condensation Cure moldmaking Material QM Skin 30 is a two-component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and very low bleed in addition to good shelf-l.. |