Material Notes:
30% Glass Reinforced, Heat Stabilized, UV Stabilized, Excellent Surface Properties
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183
Water Absorption 0.30 %
0.30 %
Sim. To ISO 62
Moisture Absorption 0.150 %
0.150 %
Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
Sim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
Sim. To ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 130 MPa
18900 psi
ISO 527-1/-2
Elongation at Break 2.4 %
2.4 %
ISO 527-1/-2
Tensile Modulus 9.90 GPa
1440 ksi
ISO 527-1/-2
Charpy Impact Unnotched 4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
4.50 J/cm²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
0.900 J/cm²

@Temperature -30.0 °C
4.28 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
22.2 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Dielectric Constant 3.9

@Frequency 1.00e+6 Hz
3.9

@Frequency 1.00e+6 Hz
IEC 60250
4.1

@Frequency 100 Hz
4.1

@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0015

@Frequency 100 Hz
0.0015

@Frequency 100 Hz
IEC 60250
0.016

@Frequency 1.00e+6 Hz
0.016

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 275 V
275 V
IEC 60112