Material Notes:
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) technology. Nyrim® is a registered trademark.Information provided by the manufacturer, Brueggemann Chemical.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.6 %
1.6 %
DIN 53714: 23°C, 50% Relative Humidity
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
ISO 868
Tensile Strength, Ultimate 22.0 MPa
3190 psi
ISO 527
Elongation at Break 420 %
420 %
ISO 527
Modulus of Elasticity 0.229 GPa
33.2 ksi
ISO 527
Flexural Modulus 0.241 GPa
35.0 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 214 °C
417 °F
DSC
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+9 ohm-cm
2.00e+9 ohm-cm
DIN 53482
Surface Resistance 2.00e+8 ohm
2.00e+8 ohm
DIN 53482
Dielectric Constant 4.8

@Frequency 1e+6 Hz
4.8

@Frequency 1e+6 Hz
DIN 53483
15.4

@Frequency 50 Hz
15.4

@Frequency 50 Hz
DIN 53483
Dielectric Strength 14.0 kV/mm
356 kV/in
DIN 53481
Dissipation Factor 0.10

@Frequency 1e+6 Hz
0.10

@Frequency 1e+6 Hz
DIN 53483
Comparative Tracking Index 600 V
600 V
DIN IEC 112 / VDE 030 t1