Material Notes:
Information provided by Domo.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Melt Flow 2.0 g/10 min
2.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Modulus 1.10 GPa
160 ksi
ISO 527-2
Izod Impact, Notched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
partial; ISO 180/1A
7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
9.00 kJ/m²

@Temperature -20.0 °C
4.28 ft-lb/in²

@Temperature -4.00 °F
ISO 180/1A
13.0 kJ/m²

@Temperature 0.000 °C
6.19 ft-lb/in²

@Temperature 32.0 °F
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point 163 °C
325 °F
ISO 3146
Vicat Softening Point 60.0 °C
140 °F
B50 (50N); ISO 306
148 °C
298 °F
A50 (10N); ISO 306