Material Notes:
AFFINITY™ EG 8200G Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. It exhibits high flexibility and elasticity. It can be utilized in monolayer cast film and in blends with other polyolefins to enhance clarity, sealability and toughness of the structure.Information provided by Dow
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
ASTM D792
Mooney Viscosity 8.0

@Temperature 121 °C
8.0

@Temperature 250 °F
ML 1+4; ASTM D1646
Melt Flow 5.0 g/10 min
5.0 g/10 min
Melt Flow Ratio = 7.5 (I<sub>10</sub>/I<sub>2</sub>); ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength, Ultimate 6.21 MPa
900 psi
ASTM D638
Tensile Strength, Yield 1.59 MPa
230 psi
ASTM D638
4.14 MPa
600 psi
100% Secant; ASTM D638
Elongation at Break >= 1000 %
>= 1000 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 63.0 °C
145 °F
Dow Method
Vicat Softening Point <= 45.0 °C
<= 113 °F
ASTM D1525