Material Notes:
AIM® 4900 advanced styrenic resin for extrusion and thermoforming applications is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatures than ABS. When used unmodified for the manufacture of food contact articles AIM 4900 complies with the US Food, Drug and Cosmetic Act and Food Additive Regulations 21 CFR 177.1640. The statute and regulations should be consulted for complete details.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 15.9 MPa
2310 psi
ASTM Data
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM Data
Elongation at Break 40 %
40 %
ASTM Data
Tensile Modulus 1.79 GPa
260 ksi
ASTM Data
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM Data
Impact Test 23.7 J

@Temperature 23.0 °C
17.5 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature 20.0 °C
45.0 µin/in-°F

@Temperature 68.0 °F
ASTM data
Vicat Softening Point 101 °C
214 °F
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Optical Properties Metric English Comments
Gloss 85 %
85 %
Gardner Gloss, 60°