Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.79 GPa | 260 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR7020 ASA ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific) ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY FXW710SK ASA General purpose injection molding ASA with Visual Fx sparkle effect. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific) Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied.. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM D638 |
Ravago Manufacturing Americas Hylac® LG35 Low Gloss ABS Acrylonitrile Butadiene Styrene, low gloss ABS.Information provided by Ravago. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR7520 ASA General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM D638 |
Total 965E Polystyrene
(discontinued **) Polystyrene 965E is a high-impact polystyrene. The extruder will see that 965E produces sheet with a dull matte finish and superior wetting tension to meet the printers needs.965E is specially desig.. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM Data |
Dow Isoplast® 202 Polyurethane (PUR-RT), Impact Modified
(discontinued **) ISOPLAST® 202 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois.. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM D638 |
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 1.79 GPa @Thickness 3.20 mm |
260 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM D638 |
Spartech SolarKote® /ABS Weatherable Sheet Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM D 638 |
Styrolution PS 7120 HIPS Excellent ESCR to foodstuffs and PUR foamsGood low temperature impact strengthHigh relative stiffness/potential to down gauge sheetUL Classification 94 HBInformation provided by Styrolution |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM D 638 |
Styrolution PS 7800 HIPS Extremely high surface glossGood processabilityUL Classification 94 HBInformation provided by Styrolution |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM Data |
Styron Magnum™ 2642 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 1.79 GPa @Thickness 3.20 mm |
260 ksi @Thickness 0.126 in |
1 mm/min, Injection Molded; ASTM D638 |
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp.. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM Data |
Styron Magnum™ 348 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM D638 |
Total PPH 3662 Polypropylene Homopolymer, Fiber Grade, for Staple Fiber, Multifilament Yarns and Slit Tape Fading Resistance TOTAL Polypropylene 3662 is formulated to resist gas fading while maintaining excellent processing stabilityProcess Stability. 3662 features excellent processability and the good.. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM D638 |
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM Data |
Dow AIM® 4900 High Impact Styrenic Resin AIM® 4900 advanced styrenic resin for extrusion and thermoforming applications is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss.. |
|||
Tensile Modulus | 1.79 - 1.98 GPa | 260 - 287 ksi | ASTM D638 |
3D Systems Accura® Xtreme Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systemsApplicationsForm, fit and function prototypesDurable AssembliesSnap fit assembliesTough enclosuresConsumer electronic componentsMaster patte.. |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM D638 |
Arkema Group Solarkote® H300 Acrylic Superior UV protection, Adhesion to HIPS, ASTM Classification PMMA 0233V3Information provided by Arkema Group |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM D638 |
Quadrant EPP Quadrant CPVC - ASTM D1748, Cell Classification (ASTM Product Data Sheet) |
|||
Tensile Modulus | 1.79 GPa | 260 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific) ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL. |