Material Notes:
BETAMATE™ 73705 is a one-part moisture curing polyurethane trim adhesive. It is formulated to provide adhesion to electro galvanized steel, phosphated steel, E-coated steel, and trim materials used in headliner systems.Information provided by Dow
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Solids Content 99 %
99 %
Viscosity Measurement 65 - 120
65 - 120
[sec], Flow Rate (0.104" orifice, 0.7 oz, 60psi)
Collected Volatile Condensable Material 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Cured
Elongation at Break 100 %
100 %
Cured
Modulus of Elasticity 0.00310 GPa
0.450 ksi
Cured
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 23.3 °C
24.0 hour

@Temperature 74.0 °F
50% RH
Descriptive Properties Value Comments
Volume Expansion % 20
Cured
Users viewing this material also viewed the following: