Dr. D. Mueller Flexiso® DMD FI 14010 00100 Polyester Electrical Insulation

Category Polymer , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer Dr. D. Mueller
Trade Name Flexiso® DMD
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dr. D. Mueller Flexiso® DMD FI 14010 00100 Polyester Electrical Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Structure: Flexiso® DMD, FI 14010 00100 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with an impregnated high temperature resin.Characteristics: Flexiso® DMD, FI 14010 00100 is characterised by very good electrical and mechanical properties, as well as low moisture absorbtion and good chemical resistance. The smooth surface allows the material to be processed on automatic feeding machines and demonstrates very good adhesion properties to impregnating and trickle. Flexiso® DMD, FI 14010 00100 is used for applications in the Insulation Class F (155 °C).Application: Flexiso® DMD, FI 14010 00100 is used, for example, in the manufacture of electric motors as slot and phase insulations, slot wedges and spacers and in the manufacture of transformers as layer insulation as well as insulating layers in various electrical devices.Delivery Form: Flexiso® DMD, FI 14010 00100 is delivered in rolls (max. width 1260 mm) and tapes (from 10 mm width). Other formats include, blanks, stamped or moulded parts in accordance with customer requirements and with self adhesive.Storage Conditions: Flexiso® DMD, FI 14010 00100 is storable for an unlimited period under normal conditions (20 °C, 50% RH). The material should be protected from damp, lack of moisture, direct sunlight and UV radiation exposure as well as any protected heat effects.Information provided by Dr. D Mueller
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
100 g/m2; IEC 626
Thickness 85.0 - 115 microns
3.35 - 4.53 mil
IEC 626
Linear Mold Shrinkage >= 0.015 cm/cm
>= 0.015 in/in
Linear Mold Shrinkage, Transverse >= 0.015 cm/cm
>= 0.015 in/in
Mechanical Properties Metric English Comments
Film Elongation at Yield, MD 12 %
12 %
Film Elongation at Yield, TD 20 %
20 %
Film Tensile Strength at Break, MD >= 55.0 MPa
>= 7980 psi
55 N/10mm
Film Tensile Strength at Break, TD >= 35.0 MPa
>= 5080 psi
35 N/10mm
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 155 °C
311 °F
IEC 216
Electrical Properties Metric English Comments
Dielectric Breakdown >= 4000 V
>= 4000 V
IEC 626
Descriptive Properties Value Comments
Color Light Blue
Polyester Film (µm) 23
IEC 626