DuPont Appeel® LSR11D542 Lidding Sealant Resin

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Appeel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Appeel® LSR11D542 Lidding Sealant Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Appeel® LSR11D542 is a modified ethylene vinyl acetate copolymer resin designed to function as a peelable sealing layer for lidding and pouch applications. It provides a peelable seal and a "whitening effect" upon peeling from polyethylene and polyethylene copolymers, as well as uncoated Tyvek®. Appeel® LSR11D542 is available in pellet form for use in conventional extrusion or coextrusion equipment designed to process polyethylene resins into blown or cast films. Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Melt Flow 2.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 105 °C
221 °F
DSC; ASTM D3418
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Processing Properties Metric English Comments
Rear Barrel Temperature 100 °C
212 °F
Blow Film
Middle Barrel Temperature 150 °C
302 °F
Blow Film
Front Barrel Temperature 210 °C
410 °F
Blow Film
Adapter Temperature 220 °C
428 °F
Blow Film
Die Temperature 220 °C
428 °F
Blow Film