Material Notes:
Bynel® Series 4200 resins are anhydride-modified low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. Bynel® 42E703 is specifically designed for high bonding performance with EVOH in high-speed coextrusion coating or laminating applications. They can also be used in cast film applications. Physical properties of Bynel® Series 4200 resins are typical of low-density polyethylene resins with similar density and melt index values.Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Melt Flow 5.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 96.0 °C
205 °F
Freezing Point, DSC; ASTM D3418
105 °C
221 °F
DSC; ASTM D3418
Vicat Softening Point 80.0 °C
176 °F
ASTM D1525
Processing Properties Metric English Comments
Rear Barrel Temperature 120 °C
248 °F
For coextrusion with EVA or EVOH.
Middle Barrel Temperature 220 °C
428 °F
For coextrusion with EVA or EVOH.
Front Barrel Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.
Adapter Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.
Die Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.