Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Die Temperature = 235 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 235 °C
455 °F
For film or coating with EVA or EVOH.
DuPont Bynel® 21E553 Adhesive Resin  (discontinued **)
Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in..
Die Temperature 235 °C
455 °F
DuPont Bynel® 30E699 Adhesive Resin  (discontinued **)
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Die Temperature 235 °C
455 °F
DuPont Bynel® 39E622 Adhesive Resin  (discontinued **)
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Die Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.
DuPont Bynel® 41E623 Adhesive Resin  (discontinued **)
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
Die Temperature 235 °C
455 °F
Extrusion Coating
DuPont Appeel® LSR11N704 Lidding Sealant Resin  (discontinued **)
Appeel® 11N704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable seal..
Die Temperature 235 °C
455 °F
DuPont Bynel® 3126 Adhesive Resin
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce..
Die Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.
DuPont Bynel® 41E687 Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
Die Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.
DuPont Bynel® 42E703 Adhesive Resin
Bynel® Series 4200 resins are anhydride-modified low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Die Temperature 235 °C
455 °F
DuPont Bynel® 30E670 Adhesive Resin
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Die Temperature 235 °C
455 °F
Extrusion Coating
DuPont™ Appeel® 20D828 Ethylene Acrylate
Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temp..
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E533 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail..
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E830 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Die Temperature 235 °C
455 °F
Cast Film/Sheet Processing
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 4033 Anhydride Modified HDPE
BYNEL® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process..
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 4140 Anhydride Modified LLDPE
BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi..
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E710 Anhydride Modified LLDPE
BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi..
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E762 Anhydride Modified LLDPE
BYNEL® 41E762 is an anhydride-modified, linear low-density polyethylene (LLDPE) resin. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextru..
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E850 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E662 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E725 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E803 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E806 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Die Temperature 235 °C
455 °F
Extrusion Coating
DuPont™ Elvaloy® AC 12024S Ethylene Methyl Acrylate
Elvaloy® AC 12024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®..
Die Temperature 235 °C
455 °F
Cast Film/Sheet Processing
DuPont™ Surlyn® 1707 Sodium Ionomer
Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t..
Die Temperature 235 °C
455 °F
Cast Film/Sheet Processing
DuPont™ Surlyn® 2601B Sodium Ionomer
Surlyn® 2601B is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer ..
Die Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.
DuPont Bynel® 50E662 Adhesive Resin  (discontinued **)
Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E662 are based on polypropylene random copolymers. They are available in pellet form for use in conventional extrusion an..
Die Temperature 235 °C
455 °F
Extrusion Coating
DuPont Appeel® LSR11D625 Lidding Sealant Resin  (discontinued **)
Appeel® LSR11D625 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals ..
Die Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.
DuPont Bynel® 50E631 Adhesive Resin  (discontinued **)
Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E631 is based on polypropylene homopolymer. They are available in pellet form for use in conventional extrusion and coextru..
Copyright © lookpolymers.com All Rights Reserved