Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 96.0 °C | 205 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 1302 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
(discontinued **) 13 wt% Methacrylic Acid.Nucrel® 1302 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process po.. |
|||
Melting Point | 96.0 °C | 205 °F | Exxon Method |
ExxonMobil Escorene® LD-612 EVA Injection Molding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer resin designed for molding and extrusion applications requiring low temperatures, flexibility and toughness. This re.. |
|||
Melting Point | 96.0 °C | 205 °F | Exxon Method |
ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Designed to be blended with a suitable masterbatch .. |
|||
Melting Point | 96.0 °C | 205 °F | ASTM D3418 |
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high .. |
|||
Melting Point | 96.0 °C | 205 °F | DSC; ASTM D3418 |
DuPont™ Surlyn® NWL Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® NWL is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Film produced from this resin is .. |
|||
Melting Point | 96.0 °C | 205 °F | ASTM D3418 |
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Melting Point | 96.0 °C | 205 °F | ASTM D3418 |
LyondellBasell Microthene® G MU76300 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Melting Point | 96.0 - 180 °C | 205 - 356 °F | |
Indium Corp. Indalloy 105 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 96.0 - 133 °C | 205 - 271 °F | |
Indium Corp. Indalloy 72 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 96.0 - 135 °C | 205 - 275 °F | |
Indium Corp. Indalloy 74 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 96.0 - 137 °C | 205 - 279 °F | |
Indium Corp. Indalloy 81 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 96.0 °C | 205 °F | ISO 3146 |
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene h.. |
|||
Melting Point | 96.0 °C | 205 °F | DSC |
Silon Tabond 2005 Adhesive Resin TABOND 2005 is a plastomer modified with maleic anhydride functional groups.Characteristics: • Strong adhesion to aminosilane treated glass, Nylon, EVOH, PET, PBT, PC, aluminium, copper, brass .. |
|||
Melting Point | 96.0 °C | 205 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Bynel® 42E703 Adhesive Resin Bynel® Series 4200 resins are anhydride-modified low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 96.0 °C | 205 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 2116 AC Ethylene and 16% Ethyl Acrylate Copolymer Elvaloy® 2116 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for specialty tubing. The material also.. |
|||
Melting Point | 96.0 °C | 205 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties.. |
|||
Melting Point | 96.0 °C | 205 °F | ASTM D3417- ISO 3146 |
DuPont Elvax® 770 Ethylene Vinyl Acetate DuPont™ Elvax® 770 is a low BHT anti-oxidant ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications: Elvax® 770 resins can be used for the following application.. |
|||
Melting Point | 96.0 °C | 205 °F | ASTM D3417- ISO 3146 |
DuPont Surlyn® 1650SB DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to .. |
|||
Melting Point | 96.0 °C | 205 °F | TRN-14 |
Tipco Tipcolite® TPF 1115 - Unreinforced Thermoset Phenolic Resin, 43 mm Norton Flow with 9% Hexamine Unreinforced Phenolic Resin having 43mm Norton Flow, in Powder FormApplications: Automotive & IndustrialProcessing: BrakeliningInformation provided by the Manufacturer, Tipco Industries Ltd.,
India... |
|||
Melting Point | 96.0 °C | 205 °F | by DSC; ASTM D3418 |
Westlake EMAC® Plus SP1305 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1305 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1305 is.. |
|||
Melting Point | 96.0 °C | 205 °F | DSC; ASTM D3418 |
Westlake Tymax™ GA7501 Anhydride Modified Acrylate Copolymer (Developmental) Westlake GA7501 is an anhydride modified acrylate copolymer for extrusion coating and cast film tie-layers. This resin is designed to function as a coextruded tie-layer in multilayer applications wh.. |
|||
Melting Point | 96.0 °C | 205 °F | DTA |
DuPont™ Surlyn® 9520 Ionomer Resin, Zinc Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Melting Point | 96.0 °C | 205 °F | Dow Method (DSC) |
Dow AFFINITY™ PF 1140G Polyolefin Plastomer (POP) AFFINITY™ PF 1140G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to be used in a variety of demanding applications including form-fill-seal packaging and fre.. |
|||
Melting Point | 96.0 °C | 205 °F | Dow Method |
Dow AMPLIFY™ VA 400 Ethylene vinyl acetate (EVA) AMPLIFY™ VA 400 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility, clarity and low temperature sealability. It is easy to process and features functional .. |
|||
Melting Point | 96.0 °C | 205 °F | |
BASF Lucalen® A 2920 M Ethylene/Acrylate Copolymer Used in the manufacture of economical composite films of Lucalen and PE-LD, and as a primer for aluminum steel composites.Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 96.0 °C | 205 °F | |
BASF Lucalen® A 2920 M Q 225 Ethylene/Acrylate Copolymer Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 96.0 °C | 205 °F | |
BASF Lucalen® A 2910 M Ethylene/Acrylate Copolymer For coating metals such as aluminum and steel, and as a primer for composites of metal or paper with Lupolen. Contains an antioxidant.Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 96.0 °C | 205 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 20E482 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Melting Point | 96.0 °C | 205 °F | ISO 3146 |
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym.. |