DuPont™ Elvaloy® AC 1330 Ethylene Methyl Acrylate

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Extrusion Grade
Manufacturer DuPont
Trade Name Elvaloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Elvaloy® AC 1330 Ethylene Methyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvaloy® AC 1330 is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® AC 1330 Acrylate Copolymer Resin complies with Food & Drug Administration Regulation 21 CFR 175.105 -- Adhesives. This Regulation describes adhesives that may be used as components of articles intended for use in packaging, transporting, or holding food, subject to the limitations and requirements therein. Elvaloy® AC 1330 Acrylate Copolymer Resin complies with Food & Drug Administration Regulation 21 CFR 176.180 -- Components of paper and paperboard in contact with dry food, subject to the limitations and requirements therein. This Regulation describes substances that may be used as components of the uncoated and coated food-contact surface of paper and paperboard in contact with dry food (Food Type VIII, identified in 21 CFR 176.170(c) Table 1).
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792, ISO 1183
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 85.0 °C
185 °F
ASTM D3418, ISO 3146
Processing Properties Metric English Comments
Processing Temperature <= 310 °C
<= 590 °F
Feed Temperature 135 °C
275 °F
Blown Film Extrusion
Zone 2 160 °C
320 °F
Blown Film Extrusion
Zone 3 185 °C
365 °F
Blown Film Extrusion
Zone 4 185 °C
365 °F
Blown Film Extrusion
Zone 5 185 °C
365 °F
Blown Film Extrusion
Adapter Temperature 185 °C
365 °F
Blown Film Extrusion
Die Temperature 185 °C
365 °F
Blown Film Extrusion
Melt Temperature 160 - 235 °C
320 - 455 °F
Blown/Cast Film Coextrusion