Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 85.0 - 125 °C | 185 - 257 °F | |
S&E Specialty Polymers GPE2001F-ROHS PVC Application: GPE2001F-ROHS is flame retardant polyethylene compound designed for wire and cable applications. GPE2001F-ROHS complies with RoHS requirements. GPE2001F-ROHS is suitable for 75°C cont.. |
|||
Melting Point | 85.0 °C | 185 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 30707SR Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
(discontinued **) 7 wt% Acrylic Acid.Nucrel® 30707SR is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio.. |
|||
Melting Point | 85.0 °C | 185 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Appeel® LSR 1184 Modified EVA Lidding Sealing Resin
(discontinued **) Appeel® 1184 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc.. |
|||
Melting Point | 85.0 °C | 185 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 3062 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 85.0 °C | 185 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 3080 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 85.0 °C | 185 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® LD 720.92 Specialty Film Resin
(discontinued **) Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Melting Point | 85.0 °C | 185 °F | Exxon Method |
ExxonMobil Escorene® LD-720 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin designed for applications requiring outstanding heat sealability along with excellent strength p.. |
|||
Melting Point | 85.0 °C | 185 °F | Exxon Method |
ExxonMobil Escorene® LD-721 High EVA Coextrusion Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin providing outstanding heat sealability along with excellent strength, properties and clarity.App.. |
|||
Melting Point | 85.0 °C | 185 °F | Exxon Method |
ExxonMobil Escorene® LD-723 High EVA Extrusion Coating Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and.. |
|||
Melting Point | 85.0 °C | 185 °F | TRN-14 |
Tipco Tipcolite® TPF 1110 - Unreinforced Thermoset Phenolic Resin, 40mm Norton Flow with 9% Hexamine Unreinforced Phenolic Resin having 40mm Norton Flow, in Powder FormApplications: General PurposeProcessing: General PurposeInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Melting Point | 85.0 °C | 185 °F | TRN-14 |
Tipco Tipcolite® TPF 550 - Unreinforced Phenolic Resin having 41 mm Norton Flow with 9% Hexamine Unreinforced Phenolic Resin having 41mm Norton Flow, in Powder FormApplications: Foundry & RefractoryProcessing: Castings & ShellsInformation provided by the Manufacturer, Tipco Industries Ltd.,
Ind.. |
|||
Melting Point | 85.0 °C | 185 °F | DSC Peak; D33418 |
Westlake EF528 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF528 is an ethylene vinyl acetate copolymer with 18.5% VA. EF528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength .. |
|||
Melting Point | 85.0 °C | 185 °F | DSC Peak; ASTM D3418 |
Westlake Elevate™ DA528AA 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength.. |
|||
Melting Point | 85.0 °C | 185 °F | Peak, by DSC; ASTM D3418 |
Westlake Elevate™ DA528AA Ethylene Vinyl Acetate Copolymer Developmental ProductDescription: Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat s.. |
|||
Melting Point | 85.0 °C | 185 °F | DSC Peak; D33418 |
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF529 is an ethylene vinyl acetate copolymer with 18.5% VA. It contains no slip or antiblock and is designed for blown and cast films requiring excellent optics and low heat seal .. |
|||
Melting Point | 85.0 °C | 185 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating 7 wt% Acrylic Acid.Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion .. |
|||
Melting Point | 85.0 - 95.0 °C | 185 - 203 °F | DSC |
EMS-Griltech Griltex® D 1500A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 85.0 - 95.0 °C | 185 - 203 °F | DSC |
EMS-Griltech Griltex® D 1500A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 85.0 - 95.0 °C | 185 - 203 °F | DSC |
EMS-Griltech Griltex® D 1516A Heat Stabilized Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 85.0 - 95.0 °C | 185 - 203 °F | DSC |
EMS-Griltech Griltex® D 1516A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications) GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides for excellent r.. |
|||
Melting Point | 85.0 - 95.0 °C | 185 - 203 °F | DSC |
EMS-Griltech Griltex® D 1616E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 85.0 °C | 185 °F | ASTM D3418, ISO 3146 |
DuPont™ Elvaloy® AC 1330 Ethylene Methyl Acrylate Elvaloy® AC 1330 is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® A.. |
|||
Melting Point | 85.0 °C | 185 °F | D.S.C. method |
Arkema Group Orevac® 9318 Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group |
|||
Melting Point | 85.0 °C | 185 °F | Exxon Method |
ExxonMobil Escorene® LD-728 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |
|||
Melting Point | 85.0 °C | 185 °F | Exxon Method |
ExxonMobil Escorene® LD-734 High EVA Extrusion Coating Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and.. |
|||
Melting Point | 85.0 °C | 185 °F | Exxon Method |
ExxonMobil Iotek® 7030 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas.. |
|||
Melting Point | 85.0 °C | 185 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 2174 Anhydride-Modified Ethylene Acrylate Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |