Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Delrin® 500TE NC010 Acetal (POM)  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced, Impact Grade
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® 500TE NC010 Acetal (POM)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Toughened Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500TE NC010 (formerly DE20560) is a medium viscosity toughened acetal homopolymer with very low VOC emissions. Processing methods include injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.015 cm/cm
0.015 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.015 cm/cm
0.015 in/in
ISO 294-4 2577
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
cm³/10min; ISO 1133
10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.0 MPa
7540 psi
ISO 527-1/-2
Elongation at Break 35 %
35 %
Nominal; ISO 527-1/-2
Elongation at Yield 20 %
20 %
ISO 527-1/-2
Tensile Modulus 2.17 GPa
315 ksi
ISO 527-1/-2
Flexural Strength 57.0 MPa

@Strain 3.50 %
8270 psi

@Strain 3.50 %
ISO 178
Flexural Modulus 2.06 GPa
299 ksi
ISO 178
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
ISO 179/1eA
0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
288 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C
169 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Additives Lubricants
Release agent
Delivery Form Pellets
Emissions <2 mg/kg
VDA 275
Part Marking Code >POM-I<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification POM-I
ISO 1043
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved