DuPont Performance Polymers Neoprene GW M2 Polychloroprene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer DuPont Performance Polymers (Former DuPont Elastomers)
Trade Name Neoprene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Neoprene GW M2 Polychloroprene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Neoprene GW is a sulfur-modified polychloroprene stabilized with a thiuram disulfide. The crystallization rate of Neoprene GW is slightly faster than that of Neoprene GRT.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792-66
Mooney Viscosity 37 - 49

@Temperature 100 °C
37 - 49

@Temperature 212 °F
ML 1 + 4; ASTM D1646-81
Descriptive Properties Value Comments
Color Light Amber
Crystallization Rate Slow
Odor Mild, characteristic
Physical Form Chips
Storage Stability Good
May undergo some viscosity changes during storage. Store under cool conditions and keep storage time to a minimum.