Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Americas Styrenics STYRON A-TECH® 1290 High Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Americas Styrenics LLC
Trade Name STYRON A-TECH®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Americas Styrenics STYRON A-TECH® 1290 High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product CharacteristicsEasy processingGood impact resistanceESCRFood Contact CompliantUL Classification 94HBTypical ApplicationsCreamer and yot containersExtrusion/ thermoformingInformation provided by AmericasStyrenics LLC.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.2 MPa
2200 psi
ASTM D638
Tensile Strength 19.3 MPa
2800 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Tensile Modulus 2.02 GPa
293 ksi
ASTM D638
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Flexural Modulus 2.12 GPa
307 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
compression molded; ASTM D256
1.82 J/cm
3.40 ft-lb/in
injection molded; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 93.9 °C
201 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
ASTM D648
Vicat Softening Point 103 °C
217 °F
ASTM D1525