Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® FE270050 BK099 Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® FE270050 BK099 Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® FE270050 BK099 is a 30% glass reinforced, polyamide 66 resin for gas and water assisted injection molding.Information provided by DuPont
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 155 MPa

@Temperature 23.0 °C
22500 psi

@Temperature 73.4 °F
DAM; 5mm/min; ISO 527
Elongation at Break 3.0 %

@Temperature 23.0 °C
3.0 %

@Temperature 73.4 °F
DAM; ISO 527
Tensile Modulus 9.00 GPa

@Temperature 23.0 °C
1310 ksi

@Temperature 73.4 °F
DAM; ISO 527
Charpy Impact Unnotched 5.50 J/cm²

@Temperature 23.0 °C
26.2 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 261 °C
502 °F
DAM; 10°C/min; ISO 11357-1/-3
Processing Properties Metric English Comments
Melt Temperature 295 °C
563 °F
DAM; optimum; Injection Molding
285 - 305 °C
545 - 581 °F
DAM; Injection Molding
Mold Temperature 50.0 - 100 °C
122 - 212 °F
DAM; Injection Molding
80.0 °C
176 °F
DAM; Optimum; Injection Molding
Drying Temperature 80.0 °C
176 °F
DAM; Injection Molding
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM; Dehumidified Dryer; Injection Molding
Moisture Content <= 0.20 %
<= 0.20 %
DAM; Injection Molding
Descriptive Properties Value Comments
Generic PA66
Part Marking Code >PA66-(GF+MD)30<
ISO 11469
Product Category Glass Reinforced Resins
Region Available - Europe Yes
Resin Identification PA66-(GF+MD)30
ISO 1043
Users viewing this material also viewed the following: