Material Notes:
Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and access cards, in multiple use tickets and in general printing applications. It is also used for medical diagnostic test strips.Approvals: UL recognized - Product has been registered with Underwriters LaboratoriesInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 82.7 MPa
12000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 82.7 MPa
12000 psi
ASTM D882A
Film Elongation at Break, MD 115 %
115 %
ASTM D882A
Film Elongation at Break, TD 90 %
90 %
ASTM D882A
Coefficient of Friction, Dynamic 0.30 - 0.40
0.30 - 0.40
A-B; ASTM D1894
Film Tensile Strength at Break, MD 152 MPa
22000 psi
ASTM D882A
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 3.0 %

@Temperature 190 °C,
Time 300 sec
3.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Gloss 40 %
40 %
45°; ASTM D1003
45 %
45 %
60°; ASTM D1003
Transmission, Visible 23 %
23 %
TLT; ASTM D1003
Electrical Properties Metric English Comments
Dielectric Strength 197 kV/mm
5000 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dielectric Breakdown 4600 V
4600 V
1/4" electrode 500 V/sec 25°C in air; ASTM D149
Descriptive Properties Value Comments
Yield (nominal) 21793 in2/lb