DuPont Teijin Films Melinex® 329W Polyester Film, 300 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 329W Polyester Film, 300 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An opaque white film with good handling properties and a unique glossy appearance. 329W has same properties as 329 with the only exception being it is wound reverse. See the 329 datasheet for details. SLIT REELS MUST BE WOUND WITH CASTING DRUM SIDE OF FILM INSIDE REEL.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 82.7 MPa
12000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 82.7 MPa
12000 psi
ASTM D882A
Film Elongation at Break, MD 115 %
115 %
ASTM D882A
Film Elongation at Break, TD 90 %
90 %
ASTM D882A
Film Tensile Strength at Break, MD 152 MPa
22000 psi
ASTM D882A
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 1.5 %

@Temperature 190 °C,
Time 300 sec
1.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.5 %

@Temperature 190 °C,
Time 300 sec
1.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Gloss 40 %
40 %
45°; ASTM D1003
45 %
45 %
60°; ASTM D1003
Transmission, Visible 9.0 %
9.0 %
TLT; ASTM D1003