Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 339 Polyester Film, 200 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 339 Polyester Film, 200 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339 is used as a base for pressure sensitive labels, photographic printing paper, in security and access cards, in multiple use tickets and in general printing applications.Approvals: UL recognized - Product has been registered with Underwriters LaboratoriesInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 82.7 MPa
12000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 82.7 MPa
12000 psi
ASTM D882A
Film Elongation at Break, MD 115 %
115 %
ASTM D882A
Film Elongation at Break, TD 90 %
90 %
ASTM D882A
Film Tensile Strength at Break, MD 152 MPa
22000 psi
ASTM D882A
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.8 %

@Temperature 190 °C,
Time 300 sec
2.8 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Gloss 40 %
40 %
45°; ASTM D1003
45 %
45 %
60°; ASTM D1003
Transmission, Visible 12 %
12 %
TLT; ASTM D1003
Descriptive Properties Value Comments
Whiteness 100
ASTM E313-79
Yield (nominal) 9900 in2/lb
Users viewing this material also viewed the following: